Texture and formation of (Bi,Pb)-2223 phase after partial-melting and solidification in high magnetic fields

X. Y. Lu, A. Nagata, K. Watanabe, T. Nojima, D. Kamio, K. Sugawara, S. Kamada

研究成果: Conference article査読

19 被引用数 (Scopus)

抄録

We investigated the texture and formation of (Bi,Pb)-2223 phase after partial-melting and solidification in high magnetic fields. It has been found that the (Bi,Pb)-2212 grains with their c-axis parallel to the magnetic field were formed after the partial-melting and solidification in 8T magnetic field, and transformed into the (Bi,Pb)-2223 grains with c-axis alignment during the further sintering process at 840 °C without magnetic field. The conversion (Bi,Pb)-2212 grains to (Bi,Pb)-2223 grains has the heredity in grain alignment.

本文言語English
ページ(範囲)3553-3556
ページ数4
ジャーナルIEEE Transactions on Applied Superconductivity
11
1 III
DOI
出版ステータスPublished - 2001 3 1
イベント2000 Applied Superconductivity Conference - Virginia Beach, VA, United States
継続期間: 2000 9 172000 9 22

ASJC Scopus subject areas

  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics
  • Electrical and Electronic Engineering

フィンガープリント 「Texture and formation of (Bi,Pb)-2223 phase after partial-melting and solidification in high magnetic fields」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル