Measurement on contact resistance and surface profile of arcing AG contacts

Hideaki Sone, Hitoshi Sugimoto, Tasuku Takagi

研究成果: Conference article査読

2 被引用数 (Scopus)

抄録

The arc duration, the contact resistance, and the electrode surface profile were measured at every operation in order to observe the detail relationship between them. The amount of loss or gain of an electrode was also calculated from the change of the electrode surface profile. In the case where the arc duration was short and ended within the metallic phase, the contact resistance was stable and low, and the surface profile was smooth. When the arc became long duration and transited to the gaseous phase, the contact resistance increased and grooves and ridges were observed on the electrode surface after first long arc. The change was reversible, but it took several consecutive operations to recover low resistance and smooth surface.

本文言語English
ページ(範囲)105-109
ページ数5
ジャーナルElectrical Contacts, Proceedings of the Annual Holm Conference on Electrical Contacts
出版ステータスPublished - 1994
イベントProceedings of the 40th Holm Conference on Electrical Contacts - Chicago, IL, USA
継続期間: 1994 10 171994 10 19

ASJC Scopus subject areas

  • 電子材料、光学材料、および磁性材料
  • 電子工学および電気工学

フィンガープリント

「Measurement on contact resistance and surface profile of arcing AG contacts」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル