Full size internal pressure creep test for welded P91 hot reheat elbow

Isamu Nonaka, Takuya Ito, Fumio Takemasa, Kensuke Saitou, Yoshikazu Miyachi, Akigo Fujita

研究成果: Article査読

10 被引用数 (Scopus)

抄録

In order to establish a life assessment method for welded modified 9Cr-1Mo steel hot reheat elbow, an internal pressure creep test was conducted with a full size test component. As a result, the fracture mode of the component has been clarified and a life prediction method has been established. Furthermore, the appropriate creep damage detection procedures have been proposed.

本文言語English
ページ(範囲)97-103
ページ数7
ジャーナルInternational Journal of Pressure Vessels and Piping
84
1-2
DOI
出版ステータスPublished - 2007 1 1