Full size internal pressure creep test for welded P91 hot reheat piping

Isamu Nonaka, Takuya Ito, Fumio Takemasa, Kensuke Saito, Yoshikazu Miyachi, Akigo Fujita

研究成果: Article査読

抄録

In order to establish the life assessment method for the welded modified 9Cr-1Mo steel hot reheat piping, an internal pressure creep test is conducted with a full size test component. As a result, the fracture mode of the component is clarified and the life prediction method is established. Furthermore, the creep damage detection procedures are proposed.

本文言語English
ページ(範囲)31-38
ページ数8
ジャーナルWelding Research Abroad
50
6-7
出版ステータスPublished - 2004 6 1