In this paper fractography of high-purity iron cleaved at low temperatures is investigated to clarify fundamental processes without the influence of impurities and inclusions. Factors affecting the initiation and the propagation of cracks are discussed from observations of river patterns and twin traces, and it is pointed out that intersection of a deformation twin with an interface such as other twins, grain boundaries or the surface can play an important role in the initiation and propagation of cracks.

寄稿の翻訳タイトルFractography of high-purity iron cleaved at low temperature
本文言語German
ページ(範囲)75-82
ページ数8
ジャーナルPraktische Metallographie/Practical Metallography
27
2
出版ステータスPublished - 1990 2月 1

ASJC Scopus subject areas

  • 電子材料、光学材料、および磁性材料
  • 凝縮系物理学
  • 材料力学
  • 金属および合金

フィンガープリント

「Fraktographie von bei tiefen Temperaturen erzeugten Reinsteisen-Spaltflaechen」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル