This paper discusses the feasibility of non-linear eddy current method to evaluate material degradations of austenitic stainless steels associated with irradiation assisted stress corrosion cracking (IASCC). For the purpose, tensile tests at elevated temperatures are conducted using model alloys simulating radiation-induced segregation (RIS), and magnetization curves of the tensile test specimens are measured by vibrating sample magnetometer (VSM). Microstructure of magnetization of the tensile test specimens is observed by magnetic force microscopy (MFM). Finally, non-linear eddy current method is carried out for the tensile test specimens. It is shown that the 3rd higher harmonic ratio of the pick-up signal is related to the targeted nominal strain.

本文言語English
ページ(範囲)1303-1308
ページ数6
ジャーナルInternational Journal of Applied Electromagnetics and Mechanics
33
3-4
DOI
出版ステータスPublished - 2010

ASJC Scopus subject areas

  • 電子材料、光学材料、および磁性材料
  • 凝縮系物理学
  • 材料力学
  • 機械工学
  • 電子工学および電気工学

フィンガープリント

「Evaluation of susceptibility to stress corrosion cracking based on non-linear eddy current method」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル