Densification and microstructure of monolithic TiN and TiB2 fabricated by spark plasma sintering

Mettaya Kitiwan, Akihiko Ito, Takashi Goto

研究成果: Conference contribution

2 被引用数 (Scopus)

抄録

Sintering behavior of monolithic TiN and TiB2 was investigated using spark plasma sintering (SPS) at temperatures between 1673 and 2573 K. Relative density of TiN was increased from 82.3 to 96.7% while that of TiB 2 increased from 70.1 to 92.8% with increasing temperature. At temperatures between 1673 and 2273 K, TiB2 was more difficult to consolidate compare to TiN. At 2473 K, TiB2 densified rapidly to 92.8%.

本文言語English
ホスト出版物のタイトルMaterials Integration
出版社Trans Tech Publications Ltd
ページ38-41
ページ数4
ISBN(印刷版)9783037853764
DOI
出版ステータスPublished - 2012
イベントInt. Symposium of GCOE: Materials Integration, in Conjunction with the 2nd Int. Symposium on Advanced Synthesis and Processing Technology for Materials, ASPT 2011 and the 8th Materials Science School for Young Scientists, KINKEN-WAKATE 2011 - Sendai, Japan
継続期間: 2011 12 12011 12 2

出版物シリーズ

名前Key Engineering Materials
508
ISSN(印刷版)1013-9826
ISSN(電子版)1662-9795

Other

OtherInt. Symposium of GCOE: Materials Integration, in Conjunction with the 2nd Int. Symposium on Advanced Synthesis and Processing Technology for Materials, ASPT 2011 and the 8th Materials Science School for Young Scientists, KINKEN-WAKATE 2011
国/地域Japan
CitySendai
Period11/12/111/12/2

ASJC Scopus subject areas

  • 材料科学(全般)
  • 材料力学
  • 機械工学

フィンガープリント

「Densification and microstructure of monolithic TiN and TiB<sub>2</sub> fabricated by spark plasma sintering」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル