A novel approach for determining the proportions of pyrolysis and hydrolysis in the degradation of poly(ethylene terephthalate) in 18O-labeled steam

研究成果: Article査読

3 被引用数 (Scopus)

抄録

The proportions of pyrolysis and hydrolysis in poly(ethylene terephthalate) (PET) degradation were determined from the decomposition of PET in 18O-labeled steam, producing labeled and unlabeled terephthalic acid. At a 100 vol % steam concentration at 400 °C, 74% of the ester bonds were pyrolyzed and 26% were hydrolyzed, as determined by gas chromatographymass spectrometry. In addition, thermogravimetric analysis revealed the activation energy to be 199 kJ mol-1 under pyrolytic conditions, decreasing with increasing steam concentration, and reaching a minimum of 132kJmol-1 at 75vol %.

本文言語English
ページ(範囲)212-214
ページ数3
ジャーナルChemistry Letters
42
3
DOI
出版ステータスPublished - 2013

ASJC Scopus subject areas

  • Chemistry(all)

フィンガープリント 「A novel approach for determining the proportions of pyrolysis and hydrolysis in the degradation of poly(ethylene terephthalate) in <sup>18</sup>O-labeled steam」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル