Surface analysis of carbon-hydrogen bonds in diamondlike carbon films by X-ray photoelectron spectroscopy

Susumu Takabayashi, Keishi Okamoto, Tatsuyuki Nakatani, Hiroyuki Sakaue, Takayuki Takahagi

Research output: Contribution to journalArticlepeer-review

5 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Surface analysis of carbon-hydrogen bonds in diamondlike carbon films by X-ray photoelectron spectroscopy'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy