Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuel

Jun ichi Tani, Masami Mayuzumi, Nobuyoshi Hara

Research output: Contribution to journalArticlepeer-review

35 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuel'. Together they form a unique fingerprint.

Physics & Astronomy

Engineering & Materials Science

Chemical Compounds