Stress Corrosion Cracking Behavior of Granite under Pressurized High Temperature Water Environments and Crack Propagation Resistance

Toshiyuki Hashida, Akihiko Hirano, Tetsuo Shoji, Hideaki Takahashi

Research output: Contribution to journalArticlepeer-review

Fingerprint Dive into the research topics of 'Stress Corrosion Cracking Behavior of Granite under Pressurized High Temperature Water Environments and Crack Propagation Resistance'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science