Stress corrosion cracking behavior near the fusion boundary of dissimilar weld joint with alloy 182-A533B low alloy steel

Hiroshi Abe, Makoto Ishizawa, Yutaka Watanabe

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Fingerprint Dive into the research topics of 'Stress corrosion cracking behavior near the fusion boundary of dissimilar weld joint with alloy 182-A533B low alloy steel'. Together they form a unique fingerprint.