Recent characterization of steel by surface analysis methods

Research output: Contribution to journalArticlepeer-review

Abstract

Surface analysis methods, such as Auger electron spectroscopy, X-ray photoelectron spectroscopy, secondary ion mass spectrometry, glow discharge optical emission spectrometry and so on, have become indispensable to characterize surface and interface of many kinds of steel. Although a number of studies on characterization of steel by these methods have been carried out, several problems still remain in quantification and depth profiling. Nevertheless, the methods have provided essential information on the concentration and chemical state of elements at the surface and interface. Recent results on characterization of oxide layers, coated films, etc. on the surface of steel are reviewed here.

Original languageEnglish
Pages (from-to)551-557
Number of pages7
JournalTetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan
Volume82
Issue number7
DOIs
Publication statusPublished - 1996

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Physical and Theoretical Chemistry
  • Metals and Alloys
  • Materials Chemistry

Fingerprint

Dive into the research topics of 'Recent characterization of steel by surface analysis methods'. Together they form a unique fingerprint.

Cite this