Proposal of fractographic analysis method coupled with EBSD and ECCI

Taketo Kaida, Motomichi Koyama, Shigeru Hamada, Hiroshi Noguchi, Eisaku Sakurada, Tatsuo Yokoi, Kohsaku Ushioda

Research output: Contribution to journalConference articlepeer-review

Fingerprint

Dive into the research topics of 'Proposal of fractographic analysis method coupled with EBSD and ECCI'. Together they form a unique fingerprint.