Abstract
Single crystalline BaTi2O5 was prepared by a floating zone method. The single crystal was transparent having a (001) cleavage plane. The space group was C2, and the lattice parameters were a = 1.6909(9) nm, b = 0.3937(1) nm, c = 0.9419(4) nm and β = 103.12(6). The permittivity perpendicular to a (010) plane showed the maximum value of 20500 at 748 K. The permittivity perpendicular to (100) and (001) planes were about 140 and 70, respectively, independent of temperature.
Original language | English |
---|---|
Pages (from-to) | 802-804 |
Number of pages | 3 |
Journal | Materials Transactions |
Volume | 44 |
Issue number | 4 |
DOIs | |
Publication status | Published - 2003 Apr |
Keywords
- BaTiO
- Floating zone method
- Lattice parameter
- Permittivity
- Single crystal
ASJC Scopus subject areas
- Materials Science(all)
- Condensed Matter Physics
- Mechanics of Materials
- Mechanical Engineering