Precipitation behavior of a novel cobalt-based superalloy subjected to prior plastic deformations

Huakang Bian, Yunping Li, Daixiu Wei, Yujie Cui, Fenglin Wang, Shihai Sun, Kenta Yamanaka, Yuichiro Koizumi, Akihiko Chiba