Non-destructive evaluation of creep damage of Ni-based superalloy using a scanning blue laser microscope

Kuniaki Akahoshi, Kazuhiro Ogawa, Hideo Miura

Research output: Contribution to journalConference articlepeer-review

1 Citation (Scopus)

Fingerprint Dive into the research topics of 'Non-destructive evaluation of creep damage of Ni-based superalloy using a scanning blue laser microscope'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science