Nanoindentation hardness and elastic modulus of AlGaN alloys

Y. Tokumoto, H. Taneichi, Y. Ohno, K. Kutsukake, H. Miyake, K. Hiramatsu, I. Yonenaga

Research output: Chapter in Book/Report/Conference proceedingConference contribution

1 Citation (Scopus)

Fingerprint Dive into the research topics of 'Nanoindentation hardness and elastic modulus of AlGaN alloys'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science

Physics & Astronomy