Abstract

A systematic study of the mechanical deformation and failure of transparent ceramic aluminum oxynitride (AlON) has been conducted using a depth-sensitive nanoindentation technique combined with transmission electron microscopy (TEM) and Raman spectroscopy. Although discrete displacement bursts appear in the load-depth profiles at high applied forces, a detectable high-pressure phase transition has not been found by means of micro-Raman spectroscopy and TEM. Instead, a high density of dissociated 〈1 1 0〉 dislocations can be observed underneath the nanoindenters, suggesting that extensive plastic deformation takes place in the brittle ceramic at high contact pressures. Moreover, nanoindentation-induced micro-cracks oriented along well-defined crystallographic planes can also be observed, consistent with the low fracture toughness of AlON evaluated by an indentation method using Laugier's equation.

Original languageEnglish
Pages (from-to)1671-1679
Number of pages9
JournalActa Materialia
Volume59
Issue number4
DOIs
Publication statusPublished - 2011 Feb

Keywords

  • Fracture toughness
  • Nanoindentation
  • Plasticity
  • Transmission electron microscopy

ASJC Scopus subject areas

  • Electronic, Optical and Magnetic Materials
  • Ceramics and Composites
  • Polymers and Plastics
  • Metals and Alloys

Fingerprint

Dive into the research topics of 'Nanoindentation characterization of deformation and failure of aluminum oxynitride'. Together they form a unique fingerprint.

Cite this