Abstract
TiC0.5N0.5-(2∼18)vol%Mo2C-16.4 vol%Ni alloys were sintered and HIP-treated at 1723 K, and then resintered at 1823 K. The microstructure, transverse-rupture strength at room temperature and 1273 K, etc. of the alloys were studied in relation to Mo2C content. The TRS at room temperature of the resintered alloy increased with increasing Mo2C content and attained a maximum with the Mo2C content of about 10%. The TRS and resistance to deformation at 1273 K became higher with increasing Mo2C content. The discussions on these results were given.
Original language | English |
---|---|
Pages (from-to) | 301-304 |
Number of pages | 4 |
Journal | Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy |
Volume | 32 |
Issue number | 8 |
DOIs | |
Publication status | Published - 1985 Jan 1 |
Externally published | Yes |
ASJC Scopus subject areas
- Mechanical Engineering
- Industrial and Manufacturing Engineering
- Metals and Alloys
- Materials Chemistry