Iodine-induced stress corrosion cracking of zircaloy-4: Identification of critical parameters involved in intergranular to transgranular crack propagation

Virginie Francon, Marion Fregonese, Hiroshi Abe, Yutaka Watanabe

Research output: Chapter in Book/Report/Conference proceedingConference contribution

7 Citations (Scopus)
Original languageEnglish
Title of host publicationEnvironmental Degradation of Engineering Materials and Materials Engineering and Technologies, EDEMET2011
PublisherTrans Tech Publications Ltd
Pages49-56
Number of pages8
ISBN (Print)9783037853207
DOIs
Publication statusPublished - 2012
Event4th International Conference on Environmental Degradation of Engineering Materials and 5th International Conference on Materials Engineering and Technologies, EDEMET2011 - Gdansk, Poland
Duration: 2011 May 152011 May 18

Publication series

NameSolid State Phenomena
Volume183
ISSN (Print)1012-0394

Other

Other4th International Conference on Environmental Degradation of Engineering Materials and 5th International Conference on Materials Engineering and Technologies, EDEMET2011
Country/TerritoryPoland
CityGdansk
Period11/5/1511/5/18

Keywords

  • Iodine-induced stress corrosion cracking
  • Transgranular cracking
  • Zircaloy-4

ASJC Scopus subject areas

  • Atomic and Molecular Physics, and Optics
  • Materials Science(all)
  • Condensed Matter Physics

Cite this