Abstract

The Li-Mn-spinel was synthesized using hydrothermal reaction through γ-MnOOH in 0.050 to approximately 0.150 mol/l LiOH aqueous solution at 130 to approximately 170 °C. The composition of the as-precipitated Li-Mn-spinel depended on both the reaction temperature and the concentration of LiOH aqueous solution. The particle was rod-shaped and the average size was around 0.2×0.2×1 μm. The charge-discharge characteristics of the as-precipitated Li-Mn-spinel were investigated in the system of Li-Mn-spinel/EC-DEC/Li. The as-precipitated Li-Mn-spinels showed an electrochemical behavior comparable to those prepared using the conventional calcination method, and the first discharge capacity varied from 62 to 107 mAh/g depending on Li content in the spinel.

Original languageEnglish
Pages (from-to)51-56
Number of pages6
JournalSolid State Ionics
Volume133
Issue number1
DOIs
Publication statusPublished - 2000 Aug 1
Externally publishedYes

ASJC Scopus subject areas

  • Chemistry(all)
  • Materials Science(all)
  • Condensed Matter Physics

Fingerprint Dive into the research topics of 'Hydrothermal synthesis and electrochemical properties of Li-Mn-spinel'. Together they form a unique fingerprint.

Cite this