Galvanic corrosion behavior of dissimilar metal joint Zr/Ta/R-SUS 304 ULC in hot nitric acid

Mariko Mori, Seiki Terasaki, Saiko Soma, Nobuyoshi Hara, Katsuhisa Sugimoto