T1 - Full-size internal-pressure creep test for welded P91 hot reheat piping
AU - Nonaka, Isamu
AU - Ito, Takuya
AU - Takemasa, Fumio
AU - Saito, Kensuke
AU - Miyachi, Yoshikazu
AU - Fujita, Akigo
PY - 2007/1/1
Y1 - 2007/1/1
N2 - In order to establish a life assessment method for the welded modified 9Cr-1Mo steel hot reheat piping, an internal-pressure creep test was conducted with a full-size test component. As a result, the fracture mode of the component was clarified and the life prediction method was established. Furthermore, creep damage detection procedures are proposed.
AB - In order to establish a life assessment method for the welded modified 9Cr-1Mo steel hot reheat piping, an internal-pressure creep test was conducted with a full-size test component. As a result, the fracture mode of the component was clarified and the life prediction method was established. Furthermore, creep damage detection procedures are proposed.
UR - http://www.scopus.com/inward/record.url?scp=33846303247&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=33846303247&partnerID=8YFLogxK
U2 - 10.1016/j.ijpvp.2006.09.018
DO - 10.1016/j.ijpvp.2006.09.018
M3 - Article
AN - SCOPUS:33846303247
VL - 84
SP - 88
EP - 96
JO - International Journal of Pressure Vessels and Piping
JF - International Journal of Pressure Vessels and Piping
SN - 0308-0161
IS - 1-2
ER -