Fatigue behavior and fracture morphology of Zr50Al 10Cu40 and Zr50Al10Cu 30Ni10 bulk-metallic glasses

G. Y. Wang, P. K. Liaw, W. H. Peter, B. Yang, M. Freels, Y. Yokoyama, M. L. Benson, B. A. Green, T. A. Saleh, R. L. McDaniels, R. V. Steward, R. A. Buchanan, C. T. Liu, C. R. Brooks

Research output: Contribution to journalArticle

69 Citations (Scopus)

Fingerprint Dive into the research topics of 'Fatigue behavior and fracture morphology of Zr<sub>50</sub>Al <sub>10</sub>Cu<sub>40</sub> and Zr<sub>50</sub>Al<sub>10</sub>Cu <sub>30</sub>Ni<sub>10</sub> bulk-metallic glasses'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science