Abstract
Transparent Lu2Hf2O7 body was first prepared by reactive spark plasma sintering using Lu2O3 and HfO2 powders. The Lu2Hf2O7 body sintered at 1723 K for 2.7 ks had an average grain size of 230 nm. The transmittance reached 78% at 2000 nm after annealing at 1123 K for 21.6 ks.