Elastic constant measurement of Ni-base superalloy with the RUS and mode selective EMAR methods

Tetsu Ichitsubo, Hirotsugu Ogi, Masahiko Hirao, Katsushi Tanaka, Makoto Osawa, Tadaharu Yokokawa, Toshiharu Kobayashi, Hiroshi Harada

Research output: Contribution to journalArticlepeer-review

16 Citations (Scopus)

Abstract

This paper reports the elastic constants of the Ni-base single crystal superalloy (TMS-26) with a rafted (lamellar) structure having tetragonal symmetry. The elastic constants have been measured at room temperature with the resonance ultrasound spectroscopy method and the mode-selective electromagnetic acoustic resonance method. The value of the elastic constant c33 (250.4 GPa) is almost equal to that of c11 (252.5 GPa), which indicates that the rafted structure virtually has the elastic anisotropy of cubic system.

Original languageEnglish
Pages (from-to)211-215
Number of pages5
JournalUltrasonics
Volume40
Issue number1-8
DOIs
Publication statusPublished - 2002 May
Externally publishedYes

Keywords

  • Electromagnetic acoustic resonance
  • Ni-base single crystal superalloy
  • Rafted structure
  • Resonant ultrasonic spectroscopy
  • Vibration mode