Crack growth behavior for stress corrosion cracking of 690 alloy in high temperature water

Tichun Dan, Zhanpeng Lü, Jianqiu Wang, Enhou Han, Tetsuo Shoji, Wei Ke

Research output: Contribution to journalArticlepeer-review

4 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Crack growth behavior for stress corrosion cracking of 690 alloy in high temperature water'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds

Earth & Environmental Sciences