TY - JOUR
T1 - A Study on Electrolytic Corrosion of Boron-Doped Diamond Electrodes when Decomposing Organic Compounds
AU - Kashiwada, Takeshi
AU - Watanabe, Takeshi
AU - Ootani, Yusuke
AU - Tateyama, Yoshitaka
AU - Einaga, Yasuaki
N1 - Publisher Copyright:
© 2016 American Chemical Society.
PY - 2016/10/26
Y1 - 2016/10/26
N2 - Electrolytic corrosion of boron-doped diamond (BDD) electrodes after applying a high positive potential to decompose organic compounds in aqueous solution was studied. Scanning electron microscopy images, Raman spectra, and glow discharge optical emission spectroscopy revealed that relatively highly boron-doped domains were primarily corroded and relatively low boron-doped domains remained after electrolysis. The corrosion due to electrolysis was observed especially in aqueous solutions of acetic acid or propionic acid, while it was not observed in other organic compounds such as formic acid, glucose, and methanol. Electron spin resonance measurements after electrolysis in the acetic acid solution revealed the generation of methyl radicals on the BDD electrodes. Here, the possible mechanisms for the corrosion are discussed. Dangling bonds may be formed due to abstraction of OH groups from C-OH functional groups by methyl radicals generated on the surface of the BDD electrodes. As a result, the sp3 diamond structure would be converted to the sp2 carbon structure, which can be easily etched. Furthermore, to prevent electrolytic corrosion during electrolysis, both the current density and the pH condition in the aqueous solution were optimized. At low current densities or high pH, the BDD electrodes were stable without electrolytic corrosion even in the acetic acid aqueous solution.
AB - Electrolytic corrosion of boron-doped diamond (BDD) electrodes after applying a high positive potential to decompose organic compounds in aqueous solution was studied. Scanning electron microscopy images, Raman spectra, and glow discharge optical emission spectroscopy revealed that relatively highly boron-doped domains were primarily corroded and relatively low boron-doped domains remained after electrolysis. The corrosion due to electrolysis was observed especially in aqueous solutions of acetic acid or propionic acid, while it was not observed in other organic compounds such as formic acid, glucose, and methanol. Electron spin resonance measurements after electrolysis in the acetic acid solution revealed the generation of methyl radicals on the BDD electrodes. Here, the possible mechanisms for the corrosion are discussed. Dangling bonds may be formed due to abstraction of OH groups from C-OH functional groups by methyl radicals generated on the surface of the BDD electrodes. As a result, the sp3 diamond structure would be converted to the sp2 carbon structure, which can be easily etched. Furthermore, to prevent electrolytic corrosion during electrolysis, both the current density and the pH condition in the aqueous solution were optimized. At low current densities or high pH, the BDD electrodes were stable without electrolytic corrosion even in the acetic acid aqueous solution.
KW - boron-doped diamond electrodes
KW - electrolytic corrosion
KW - methyl radicals
KW - organic compounds
KW - wastewater treatment
UR - http://www.scopus.com/inward/record.url?scp=84994057018&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84994057018&partnerID=8YFLogxK
U2 - 10.1021/acsami.5b11638
DO - 10.1021/acsami.5b11638
M3 - Article
AN - SCOPUS:84994057018
SN - 1944-8244
VL - 8
SP - 28299
EP - 28305
JO - ACS applied materials & interfaces
JF - ACS applied materials & interfaces
IS - 42
ER -